CarbonX PETG+CF
CarbonX PETG+CF
CarbonX PETG+CF

CARBONX™ PETG+CF

SKU: PTG03CF102000BK00

Regular price
$120.00
Sale price
$120.00
Regular price
$0.00
Shipping calculated at checkout.

Benefits of CARBONX™ PETG+CF

  • CarbonX™ PETG+CF is a carbon fiber reinforced PETG filament enhanced with engineering-grade carbon fiber, delivering up to 2.5x greater stiffness and 20% higher strength than standard PETG — ideal for structural, functional, and end-use parts.
  • Amorphous structure giving it low, near isotropic shrinkage
  • Low moisture absorption, 3x lower than ABS
  • Very low odor while printing
  • Wide processing range from 230-270°C
  • Bambu AMS Compatible: our 750g reels fit the Bambu AMS, Creality CFS, and Anycubic ACE Pro, so you can run engineering-grade filament in your favorite material management system.
  • CarbonX™ PETG+CF requires specific processing conditions, such as higher extruder temperatures and slower cooling rates, to maintain the integrity of the carbon fibers and the matrix.
  • Carbon fiber filaments are abrasive and will accelerate wear on standard brass nozzles. A hardened steel nozzle is required for printing CarbonX PETG+CF.
Color Code: Black
Diameter:
Reel Size:
In Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials.

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CarbonX PETG+CF

CarbonX™ PETG-CF filament is made in the USA using premium PETG and engineering-grade carbon fiber. CarbonX™ PETG+CF is an improved carbon fiber reinforced PETG filament vs. the competition. This filament is ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
230-260C
140-160°C
Bed Temp
70-90C
Recommended
Heated Chamber
Not Required
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
65C for 4 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.