Benefits of Firewire FR-ABS

  • Durable and sturdy parts with highly flame-retardant, self-extinguishing properties
  • Easier to print than most industrial-grade materials
  • Made using UL94 V-0 rated base resin
Color Code: Black
Diameter:
Reel Size:
In Stock

Firewire FR-ABS

Flame retardant materials are essential across industries for minimizing fire risks, ensuring safety compliance, and improving overall reliability. Firewire FR-ABS is a premium UL94 V-0 rated ABS that allows for printing of functional prototypes and production parts. This material is ideal for printing electrical housings, connectors, or any part that requires thermal properties [up to 95°C] and flame retardant ABS characteristics.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
220-240C
140-160°C
Bed Temp
100-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
80°C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.