WearX_PA6
WearX_PA6

WearX Wear Resistant Nylon Filament

SKU: NYL16UN100500BK00

Regular price
$68.00
Sale price
$68.00
Regular price
$0.00
Shipping calculated at checkout.

Benefits of WearX Wear Resistant Nylon Filament

  • 3x Improved Wear Resistance vs. Unfilled AmideX PA6 Copolymer
  • High strength 62 MPa tensile str. with lightly lower impact / elongation vs. unfilled nylon
  • Improved chemical resistance compared to many other traditional 3D printing filaments
  • Excellent printability with a more matte surface than unfilled PA6-66 copolymers
  • Good thermal properties with a Tg of 76C, 143C HDT, and Tm of 200C
  • Ideal for 3D printing net shape or near-net shape tribological applications that were previously machined from stock shapes such as Nylatron GS MoS2 filled nylons
  • Wear resistance gradually diminishes as in-use temperatures rise and are limited in this formulation to 120C
  • Formulated for enhanced wear resistance under dry conditions, but the addition of external lubricants will extend wear-life
Color Code: Black
Diameter:
Reel Size:
Out Of Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials.

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

WearX Wear Resistant Nylon Filament

WearX PA6 has been modified for enhanced wear resistance for greatly improved wear resistance vs. standard PA6 (3X improvement!). WearX PA6 offers a harder surface, improved dimensional stability, and a matte surface appearance. This material was inspired by the need for an enhanced material specifically formulated to resist sliding and rotational wear.

End Use Tip: Ideal for 3D printing net shape or near-net shape tribological applications that were previously machined from stock shapes such as Nylatron GS MoS2 filled nylons.

Pro Tip: Wear resistance gradually diminishes as in-use temperatures rise and are limited in this formulation to 120C. WearX PA6 was formulated for enhanced wear resistance under dry conditions, but the addition of external lubricants will extend wear-life, especially at elevated temperatures and under increased loading and/or speeds (high PV’s).

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
260-275C
140-160°C
Bed Temp
80-95C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
0.2mm or Larger
0.10mm or higher
Layer Height
0.15mm or Larger
65°C for 4 hours
Drying Specs
90C for 4-6 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.