Benefits of 3DXMAX HIPS

  • Very good, strong support material
  • Prints very easily
  • Polymer doesn’t absorb moisture, no drying required!
  • Can be removed from models by hand and be dissolved away with d-limonene
  • Works perfectly with many materials, especially the industry’s workhorses like ABS and ASA.
  • This includes all of our famous composite variants of these grades, such as carbon fiber, glass fiber, and ESD-safe. B10
Color Code: Natural
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

3DXMAX HIPS

Manufactured in the USA from 100% virgin High Impact Polystyrene resin. We use state-of-the-art resins manufacturing technologies to give you the best possible printing experience. HIPS can be used for parts that require low-gloss and nearly invisible layer lines. It does not absorb moisture, so you do not need to keep it in a dry box.

Plus, it requires very little setup to achieve truly great prints in practically any 3D printer. It can also be used as an excellent break-away support for ABS and ASA or completely dissolved in d-limonene.

Precision extruded using our own formulation, this grade is a bit different than the usual HIPS used to make our model material colors. It’s formulated to be more sensitive to attack from d-limonene solvent and make a better dissolving support solution.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
220-235C
140-160°C
Bed Temp
100-110C
Recommended
Heated Chamber
Not required
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
Not needed

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.