CarbonX PLA+CF
CarbonX PLA+CF

CARBONX™ PLA+CF

SKU: PLA03CF302000BK00

Regular price
$53.40
Sale price
$53.40
Regular price
$89.00
Shipping calculated at checkout.

Benefits of CARBONX™ PLA+CF

  • Ideal for printing without a heated bed, no enclosure required
  • Bambu AMS compatible
  • Very low odor, perfect for 3D printing in home and office environments
  • Carbon fiber reinforcement increases stiffness and dimensional stability
  • Improved surface quality for aesthetic parts
  • Bambu AMS compatible
  • Strongly recommend this material to be printed through a hardened steel nozzle rather than a softer metal.
Color Code: Black
Diameter:
Reel Size:
In Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials.

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CarbonX PLA+CF

CarbonX PLA+CF is a 3D printing filament made with NatureWorks biopolymer, reinforced with carbon fiber. This material is ideal for anyone that desires high flexural modulus, excellent surface quality, dimensional stability, low density, and ease of printing. PLA+CF was developed for prototypes and applications where aesthetics, stiffness, and consistency are paramount.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
190-220 C
140-160°C
Bed Temp
23-60 C
Recommended
Heated Chamber
Not Required
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
65C for 4 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.