3DXTECH Filaments
Order 3D printing filament for all desktop printers. Try Carbon Fiber, ESD-Safe, and Glass Fiber materials manufactured in the United States by 3DXTECH.
3DXTECH Filaments
$78.00 – $195.00
CarbonX™ PP+CF is made using a specialty formulated PP copolymer and reinforced with premium high-modulus carbon fiber. This material offers ease of printing, strength & stiffness, excellent dimensional stability, and an amazing surface finish.
CarbonX™ PP+CF is made using a specialty formulated polypropylene copolymer reinforced with high-modulus chopped carbon fiber. This filament is based on a patent-pending formulation that offers improved thermal properties and low shrinkage/warp compared to competitive PP-based compounds.
The reels contain 750g of filament, but based on the very low density of PP+CF, this is the same amount of filament that would typically be found on a 1kg reel of ABS. This allows you to print light-weight and exceptionally rigid parts for medical, drones, watercraft, automotive, or any application which would benefit from a light weight, stiff, chemically resistant material.
Extruder Temp220-250°C
Bed Temp23-60°C
Heated ChamberNot required
Nozzle Specs0.4mm diameter minimumHardened Steel Nozzle
Bed AdhesionMagigoo Bed Prep
Layer Height0.25mm or higher
Drying SpecsNot needed
SupportsWater Soluble Support
Since properties can change depending on print environment and 3D model geometry and/or surface area, it is always required to do your own testing, but Polypropylene is famous for its chemical resistances to a huge range of environments including:
This material doesn’t yet have a formal SDS.
1.75mm and 2.85mm +/- 0.05mm in diameter
What Is It?
Fibers 5-10 micrometers wide made of carbon. The fibers are aligned following the axis of the material.
This, along with their physical makeup, are what give this material its excellent properties.
What Does It Do?
Carbon Fibers demonstrate a lot of desirable material properties:
How Does It Work?
Reinforcing plastic with carbon fibers produces a 3D printing filament which exhibits the best properties of both the carbon fibers and the plastic of choice.
What Is It Good For?
Ideal for any applications which require light weight and rigidity.
Carbon fiber reinforced parts, designed to use less material and save weight, is extremely popular in aerospace, civil engineering, the military, and motorsports.
This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.
Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.