3DXMAX LTS2
LTS2 Break Away Support was developed for our Gearbox™ HT2 3D Printer. This material is specifically formulated as a break away support for ABS and ASA model materials. LTS2 is capable of supporting ABS and ASA in heated build chambers up to 100°C. Suitable for open-source printers with non-heated chambers and those with chambers up to 100°C.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.