Economy PLA

SKU: PLA175BU2M

Regular price
$13.49
Sale price
$13.49
Regular price
$17.99
Shipping calculated at checkout.

Benefits of Economy PLA

  • Bambu AMS compatible
  • Low shrinkage, warping, and easy printability, PLA prints great on practically any desktop 3D printer
  • Very low odor, perfect for 3D printing in home and office environments
  • Gorgeous surface quality to make printed parts look beautiful
  • Ideal for printing without a heated bed, no enclosure required
Color Code: economy-dark-blue
Diameter:
Reel Size:
In Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials. 

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Need a larger quantity or looking for a product that's currently out of stock? Contact our Sales Team to get more information on the products you need.

Contact our Sales Team

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

ECONOMY PLA

3DXTECH Economy PLA is part of our newest line of high-quality filaments. Our PLA is known for it high quality performance and experienced users understand that performance filaments make the difference. The Economy PLA offers the same high quality performance, but for a fraction of the price.

PLA is most well-known for its ease of printing, stiffness, and extremely high visual print quality. It is ideal for prototypes, concept models, and end-use printed parts for hobbyists to industry engineers alike!

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
190-220C
140-160°C
Bed Temp
23-60C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
45C fo 4 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.

Contact Our Sales Team

Need a larger quantity or looking for a product that's currently out of stock? Complete the form below, and our sales team will reach out to assist with pricing, availability, and purchasing options.