Benefits of CARBONX™ PEI 9085+CF

  • High thermal properties, Tg of 186C and an HDT of 165C
  • Inherent flame resistance due to Ultem 9085 base resin
  • Improved stiffness and strength for structural applications
  • Excellent dimensional stability – lower CTE, warp, and shrinkage vs unfilled grades
  • Resistance to a broad range of chemicals, include automotive fluids, fully halogenated hydrocarbons, alcohols, and aqueous solutions
  • Strongly recommend this material to be printed through a hardened steel nozzle rather than a softer metal.
Color Code: Black
Diameter:
Reel Size:
In Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials. 

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Need a larger quantity or looking for a product that's currently out of stock? Contact our Sales Team to get more information on the products you need.

Contact our Sales Team

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CARBONX PEI 9085+CF

CarbonX™ CF PEI 9085 is made using Sabic Ultem™ 9085 resin and 15% high-modulus carbon fiber. This custom formulation is an excellent printing aerospace-grade material specifically formulated for our aerospace clients.

Ultem™ 9085 is FAA-approved for FST applications (Flame/Smoke/Toxicity) and meets FAR 25.853 and OSU 65/65 standards. The addition of 15% high-modulus carbon fiber allows for superior strength and stiffness while maintaining excellent dimensional stability and printability.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
365-390C
140-160°C
Bed Temp
140-160C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
140°C for 6-8 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED