THERMAX™ PEKK-A

SKU: PKK09UN101000BK01

Regular price
$550.00
Sale price
$550.00
Regular price
$0.00
Shipping calculated at checkout.

Benefits of THERMAX™ PEKK-A

  • Made with Arkema Kepstan PEKK resin — a certified, ultra-performance polyetherketoneketone polymer trusted in aerospace, oil & gas, and defense applications
  • High thermal properties with a CUT of 260°C, Tg of 162°C, and a Tm of 335°C
  • Substantially easier to 3D print than PEEK — PEKK's slower crystallization rate and lower internal stress result in better layer adhesion and a wider processing window
  • Wide processing window from 345–375°C
  • Inherently flame resistant (UL94 V-0)
  • Low smoke generation
  • Outstanding mechanical, thermal, and chemical resistances
Color Code: Black
Diameter:
Reel Size:
In Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials. 

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Need a larger quantity or looking for a product that's currently out of stock? Contact our Sales Team to get more information on the products you need.

Contact our Sales Team

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

THERMAX PEKK A

ThermaX PEKK (PolyEtherKetoneKetone) is made using Arkema Kepstan PEKK and is one of the highest-performance polymers in plastics business. A leading material in the PAEK family, PEKK has exceptionally good mechanical, thermal, and chemical resistance properties. It is also not only substantially easier to print than PEEK, it’s one of the easiest ultra-polymers to 3D print period. Developed in partnership with Arkema, a leading supplier of ultra-performance materials.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
345-375C
140-160°C
Bed Temp
120-140C
Recommended
Heated Chamber
Recommended 70-150C if possible
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED