ABScent™ ABS Filament, Ruby

Hover over image to zoom

  • Ruby ABScent™ ABS
  • Image 2
  • Image 3
$29.95

 Product Description

Ruby Red ABScent® Transparent ABS.  

ABScent™ ABS is transparent and odorless premium 3D printing filament formulated utilizing high-flow MABS [methylmethacrylate acrylonitrile butadiene styrene] resin and colorants. ABScent™ ABS offers superior mechanical properties to most ABS filaments, absent the odor. MABS is an amorphous acrylic-modified ABS polymer that has practically no odor – especially when compared to traditional ABS resins. This makes it ideal for printing in public spaces, schools, and office environments. 

Color:  Brilliant Ruby Red Translucent ABS

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Data Sheets & MSDS

Recommended Print Conditions:

  • Extruder Temp:  230 - 260°C.  In-house testing indicates best toughness and clarity above 250°C.   
  • Extruder Speed:  4000mm/min
  • Bed Temp:  90-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry
  • Support:  Our HIPS support works great to create complex parts.  Our HIPS support can be found HERE.  

 Product Reviews

You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the ABScent™ ABS Filament, Ruby to your wish list.