Ecomax® rPETG
Ecomax® rPETG is a durable material that has excellent strength while remaining flexible. The base resin used in our rPETG filament is FDA approved and has improved chemical resistance compared to PLA or ABS. It is suitable for cleaning with isopropyl alcohol as needed.
Print Recommendations

Extruder Temp
230-260°C

Bed Temp
60-90°C

Heated Chamber
Not required

Nozzle Specs
No special concerns

Bed Adhesion
Magigoo Bed Prep

Layer Height
No special concerns

Drying Specs
65°C for 4 hours

Supports
Works best with
X1 USM Water Soluble Support
Benefits of rPETG Include:
- Superior chemical resistance to ABS
- Very low odor while printing
- Amorphous structure giving it a low, near isotropic shrinkage
- Low moisture absorption, 3x lower than ABS
- Wide range of processing from 230-260°C
- Superior ductility vs. ABS

Technical Data Sheet
TDS for this material coming soon!

Safety Data Sheet
TDS for this material coming soon!
Chemical Resistance of rPETG:
Unstressed tensile bars molded of PETG exhibit good resistance to dilute aqueous solutions of mineral acids, bases, salts, and soaps, as well as aliphatic hydrocarbons, alcohols, and a variety of oils. Halogenated hydrocarbons, short chain length ketones, and aromatic hydrocarbons still dissolve or swell the plastic.

Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 230-260°C
- Bed Temp: 60-90°C
- Bed Prep: Magigoo Bed Prep Adhesive and 3DXTECH Polyimide Tape work best for us.
- Heated Chamber: Not required
- Supports: Water soluble AquaTek X1 USM works great for complex parts.
- Drying Instructions: 65°C for 4 hours.