Thermax™ HTS2 High-Temp Support Filament [9085 Break Away Support]
Our break away high-temp support filament is ideal for use in dual extruder 3D printers designed to print high-temp materials.
HTS is the premium support for our high-temp products, unlike most support filaments, which are not designed to withstand the heat required to print the top-end of performance materials.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our HTS Filament and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations
Extruder Temp
350-380°C
Bed Temp
120-160°C
Heated Chamber
Recommended
(No higher than 185°C)
Nozzle Specs
No special concerns
Bed Adhesion
Nano Polymer Adhesive
Layer Height
No special concerns
Drying Specs
120°C for 4 hours
Supports
HTS is break-away
Works ideal with the following ThermaX™ materials:
Support Removal:
- This is break-away support and does not dissolve.
- High-Temp support is best removed while printed part is still warm.
- If the finished printed part cools completely and the support removal gets too difficult, you can re-warm the part in the printer chamber or an oven not exceeding the Tg of the model material you are printing with.
Technical Data Sheet
This material doesn’t yet have a formal TDS.
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 350-380°C
- Bed Temp: 120-160°C
- Bed Prep: Nano Polymer Adhesive or Polyimide Tape gives us the best results.
- Heated Chamber: All high-temp materials print better with a heated enclosure or build environment. Enclosure temp should not exceed 185°C for our high-temp support material to remain structurally sound as a support.
- Other: Don’t use a cooling fan while printing this support.
- Drying Instructions: 120°C for 4 hours
ULTEM™ is a registered trademark of Sabic Innovative Plastics.