Flexible Filaments

Flexible Filaments

 

3DXFLEX™ TPC thermoplastic copolyester elastomer is an engineering-grade filament that offers ease of printing, excellent flexibility, good chemical resistance, and superior toughness.  This grade of flexible filament is considered to be more friendly to print with than TPU-based filaments.