3DXTECH™ ABS 3D Printing Filament

3DXTECH™ ABS, 1kg

$29.95

ABS 3D Printing Filament, 1kg Reel

3DXTech™ ABS is made in the USA using 100% virgin resin and colorants - precision extruded onto 1kg reels (2.2 lbs.).  The filament is then vacuum-sealed with desiccant to protect it from moisture.  

Print industrial-grade ABS parts with Gearbox™ HT2 High-Temp 3D Printer.  Check it out HERE. 

Filament diameter specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  220-240°C, Ideal 230°C
  • Bed Temp:  100-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry
  • Support Material:  We recommend our AquaTek™ water soluble support - HERE
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.