3DXTECH™ ABS
3DXTECH™ ABS (Acrylonitrile Butadiene Styrene) is one of the most widely used 3D printer filaments on the market, and for good reason. Our ABS is a premium mix specially formulated for 3D printing. It has excellent mechanical properties and printability, giving this material’s parts durability and a less brittle quality than other similar polymers.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our ABS filament and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations
Extruder Temp
220-240°C
Bed Temp
100-110°C
Heated Chamber
Recommended
Nozzle Specs
No special concerns
Bed Adhesion
Magigoo Bed Prep
Layer Height
No special concerns
Drying Specs
80°C for 4 hours
Supports
Works best with
X1 USM Water Soluble Support
Benefits of 3DXTECH™ ABS:
- Durable and sturdy parts off practically every 3D printer on the market
- Easier to print than most industrial-grade materials
- Parts can be smoothed with acetone vapors
- Many colors to make your models pop!
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 220-240°C
- Bed Temp: 100-110°C
- Bed Prep: Magigoo Bed Prep Adhesive and 3DXTECH Polyimide Tape work best for us.
- Heated Chamber: Recommended, a chamber helps reduce warping.
- Supports: Water soluble AquaTek X1 USM works great for complex parts.
- Drying Instructions: 80°C for 4 hours.