PLA 3D Printing Filament

ECOMAX® PLA, 3D Filament, 1 kg

$29.95

ecomax_pla_filament

ECOMAX® PLA Biopolymer is made in the USA using 100% virgin PLA Naturworks biopolymer resin and premium colorants.  Our filament is precision extruded onto 1kg reels (2.2 lbs) and then vacuum-sealed with desiccant to protect it from moisture.  

4th of July Sale!  Save 25% on our 1kg reels of PLA.  Use coupon code 25%Off4th2019 when you check out.  
 
This filament is ideal for use with practically all desktop printers, such as Makerbot, Reprap, Printrbot, Prusa, UP / Afinia, Flashforge, Anet, Creality, Lulzbot, Makergear, Ultimaker, or any other printer accepting 1.75mm or 3.0mm filament.
 
Check out the ideal support material for dual extruder printers:  AquaTek Water Soluble Support (HERE).  Works great with PLA and a wide array of materials.  
 
Filament diameter specs:
  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  190-220°C
  • Bed Temp:  23-60°C [No Heated Bed Required]
  • Bed Prep:  3DXTech Blue Painters Tape, Hairspray, Glue Stick

New Colors!  The closest Pantone matches for our new colors are:

  • Red: Pantone 1795C 
  • Blue: Pantone 2152C
  • Green: Pantone 348C
  • Yellow: Pantone 121C
  • Orange: Pantone 1485C
  • Cool Grey: Pantone 8C