ECOMAX® PLA Biopolymer is made in the USA using 100% virgin PLA Naturworks biopolymer resin and premium colorants. Our filament is precision extruded onto 200g reels and then vacuum-sealed with desiccant to protect it from moisture.
This filament is ideal for use with practically all desktop printers, such as Makerbot, Reprap, Prusa, UP / Afinia, Flashforge, Anet, Creality, Makergear, or any other printer accepting 1.75mm filament.
Check out the ideal support material for dual extruder printers: AquaTek™ Water Soluble Support (HERE). Works great with PLA and a wide array of materials.
Filament diameter specs:
- 1.75mm +/- 0.05mm
Recommended Print Conditions:
- Extruder Temp: 190-220°C
- Bed Temp: 23-60°C [No Heated Bed Required]
- Bed Prep: 3DXTech Blue Painters Tape, Hairspray, Glue Stick
New Colors! The closest Pantone matches for our new colors are:
- True Red: Pantone 1795C
- True Blue: Pantone 2152C
- True Green: Pantone 348C
- True Yellow: Pantone 121C
- True Orange: Pantone 1485C
- Cool Grey: Pantone 8C