Flame Retardant UL-94 V-0 Rated ABS

Firewire® Flame Retardant PC/ABS, 1kg

$78.00

Flame Retardant ABS FilamentFirewire® Flame Retardant PC-ABS 3D Printing Filament, 1kg Reel

Firewire® FR PC-ABS (polycarbonate + ABS alloy) is made using a premium UL94 V-0 rated PC-ABS.  Our FR PC-ABS has higher strength and thermal resistance (HDT) than ABS and is supplied on 1kg reels (2.2 lbs.) reels.  This filament is ideal for applications that require UL94 V-0 self-extinguishing characteristics.  

Filament diameter specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  265-285°C, Ideal 270°C
  • Bed Temp:  110 - 120°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.  

*This is the UL94 rating of base resin we use to make Firewire® FR PC-ABS Filament.