PLA 3D Printing Filament

ECOMAX® PLA

$29.95 $24.95
(You save $5.00)

ecomax_pla_filament

ECOMAX® PLA Biopolymer is made in the USA using 100% virgin PLA Naturworks biopolymer resin and premium colorants.  Our filament is precision extruded onto 1kg reels (2.2 lbs) and then vacuum-sealed with desiccant to protect it from moisture.  

This filament is ideal for use with practically all desktop printers, such as Makerbot, Reprap, Prusa, Ender, Flashforge, Anet, Creality, Lulzbot, Makergear, Ultimaker, or any other printer accepting 1.75mm or 3.0mm filament.

Check out the ideal support material for dual extruder printers:  AquaTek Water Soluble Support (HERE).  Works great with PLA and a wide array of materials.  

Filament diameter specs:
  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  190-220°C
  • Bed Temp:  23-60°C [No Heated Bed Required]
  • Bed Prep:  3DXTech Blue Painters Tape, Hairspray, Glue Stick

New Colors!  The closest Pantone matches for our new colors are:

  • Red: Pantone 1795C 
  • Blue: Pantone 2152C
  • Green: Pantone 348C
  • Yellow: Pantone 121C
  • Orange: Pantone 1485C
  • Cool Grey: Pantone 8C