ThermaX™ PES (PESU) 3D Printing Filament
Polyether Sulfone (PES or PESU) is a high-temperature aromatic sulfone polymer that exhibits exceptional thermal, mechanical, and chemical resistance properties. PES is part of the PAES (Poly Aryl Ether Sulfone) family of polymers, which includes PSU, PES, and PPSU. ThermaX™ PES is an amorphous polymer and has excellent dimensional stability and creep resistance.
PES has higher temperature resistance and toughness than Ultem™ 1010, offering the ability to print parts with higher mechanical properties at elevated temperature.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our PES filament and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations
Extruder Temp
340-390°C
Bed Temp
140-160°C
Heated Chamber
Recommended
Nozzle Specs
No special concerns
Bed Adhesion
Nano Polymer Adhesive
Layer Height
No special concerns
Drying Specs
120°C for 4 hours
Supports
Works best with HTS break-away support
Benefits of ThermaX™ PES (PESU):
- Very high thermal properties superior to Ultem™ 1010
- Glass Transition Temp of 228°C
- High Environmental Stress Crack Resistance (ESCR)
- Sterilization capable, including EtO gas, radiation, steam autoclaving, plasma, dry heat and cold sterilization
- Exceptional strength and modulus, even at elevated temperatures
- Resists most common automotive fluids including gasoline, antifreeze, transmission fluids, motor oils, power steering fluid, windshield washer fluid (ESCR, 24 hrs, 100°C)
- Inherently flame retardant with low smoke evolution and low smoke toxicity
- Excellent dimensional stability with low creep sensitivity, low and uniform coefficient of thermal expansion, and highly reproducible part-to-part dimensions.
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
1.37g/cm3 density
Recommended Print Settings:
- Extruder: 340-390°C
- Bed Temp: 140-160°C
- Bed Prep: Nano Polymer Adhesive and 3DXTECH Polyimide Tape work best for us.
- Heated Chamber: Recommended
- Supports: ThermaX™ HTS High-Temp Support is designed specifically to work with high-temp materials like this one.
- Other: No cooling fan and print speeds of 16 mm/s as a starting point.
- Drying Instructions: 120°C for 4 hours.