PLA Plastic Pellets

PLA Pellets

$16.00
Lead Time:
3 to 5 business days

PLA Pellets

Ideal for home extrusion enthusiasts.  Make your own high-performance PLA filament with a home-extruder such as Filabot, Filastruder, and Noztek.  This is the same PLA that we use for our ECOMAX(R) PLA Filament.

Please note:  Additional shipping charges may apply on orders over 10 pounds.

Processing Recommendations:

  • Pre-dry before extrusion at 60°C for 4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  170 - 190°C