ABS Pellets
Use 3DXTECH ABS Pellets to make your own high-performance ABS filament with a home-extruder or when using a pellet-fed printer.
Processing Recommendations:
- Pre-dry before extrusion at 80°C for 2-4 hours. A toaster oven works fine for this. Do your family a favor and do not dry the resin in your kitchen oven! (Wet material will extrude with bubbles present in the filament. If this happens, dry the resin more before processing.)
- Extrusion Temp: 190 – 210°C