PVA Plastic Pellets

PVA Water Soluble Support Pellets

$48.00
Lead Time:
3 to 5 business days

PVA Water Soluble Support Pellets

Ideal for home extrusion enthusiasts.  Make your own high-performance PVA support filament with a home-extruder such as Filabot, Filastruder, and Noztek.  

Please note:  Additional shipping charges may apply on orders over 10 pounds.

Processing Recommendations:

  • Pre-dry before extrusion at 50°C for 4-6 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  150 - 170°C depending on your extruder set-up.
  • Do not cool using water tanks - this is a water soluble material and will dissolve in the water.