AquaTek X1 Advanced USM Universal Support Material

$90.00$170.00

4 interest-free payments with Klarna-Logo-Icon  Learn More

AquaTek™ X1 Advanced USM [Universal Support Material] is an advanced water-soluble support filament that was formulated specifically for printing complex parts. This material is compatible with the widest variety of model materials [PLA, ABS, NYLON, Carbon Fiber, Glass Fiber, and more!] and then it safely washes away in warm water so you don’t destroy your part removing the support.

SKU: Select options above Brand: AquaTek™ Categories: ,

AquaTek™ X1 Advanced USM Universal Support Material

Our AquaTek™ X1 Advanced USM Universal Support Material is an all-new, highly advanced universal water soluble support formulated specifically for printing complicated parts. AquaTek™ X1 Advanced USM is readily dissolved in warm water and has excellent adhesion to the broadest range of materials, including our popular advanced composites like CarbonX™ Carbon Fiber Nylons and FibreX™ Glass Fiber Nylons.

Ext Temp 1

Extruder Temp
245-265°C

Bed Temp

Bed Temp
60-90°C

Chamber Temp

Heated Chamber
Not required

Nozzle Settings

Nozzle Specs
No special concerns

Bed Adhesion

Bed Adhesion
Magigoo Bed Prep
Nano Polymer Adhesive

Layer Height

Layer Height
No special concerns

Drying Filamen

Drying Specs
65°C for 2-4 hours

Water Soluble Support

Supports
X1 USM is water soluble

Benefits of AquaTek™ X1 Advanced USM:

  • Readily soluble in warm water
  • Eco-friendly and safe to dispose in house or office drains
  • Ideal support material for the widest array of materials, including many which are infamous for being difficult to support!
  • Low moisture absorption while exposed to the air during printing, getting less tacky over time than similar support materials

Compatible Materials:

  • AquaTek™ X1 Advanced USM really is our most compatible support material, it works excellent with all the following and more:
  • PLA, ABS, ASA, PETG, Nylons, and flexible filaments like TPC, TPU, and COPE.
  • This includes all of our famous composite variants of these grades, such as carbon fiber, glass fiber, and ESD-safe.

Recommended Support Removal Techniques:

Break away excess support material that’s easily accessible. This reduces dissolution time (more support material = a longer time to dissolve).

Submerge the part in warm water. Hot tap water is typically 38-49°C, which is more than adequate for dissolving AquaTek™ X1 Advanced USM. Please be safe with hot water!

Agitating and stirring the water reduces dissolution time further, either with mechanical agitation or a sonic cleaning bath system. Re-heat or replace the warm water as it cools off for as long as you still see support material un-dissolved.

Residue is ecologically safe and can be disposed of down a home or office drain. Rinse thoroughly with fresh, warm water.

X1 Water Soluble Support Filament

Filament Specifications:

1.75mm and 2.85mm +/- 0.05mm in diameter

Recommended Print Settings:

  • Extruder: 245-265°C
  • Bed Temp: 60-90°C
  • Bed Prep: Magigoo Bed Prep Adhesives, Nano Polymer Adhesive, or Polyimide Tape gives us the best results.
  • Heated Chamber: Not required, but often helpful. Enclosure temp should not exceed 120°C for X1 USM
  • Other: AquaTek™ Advanced X1 Advanced USM will absorb moisture from ambient humidity, therefore best practice is to store filament in a sealed container while not in use.
  • Drying Instructions: 65°C for 2-4 hours

Questions?