CF15 PP Pellets [15% Carbon Fiber Polypropylene]

Ideal for home extrusion enthusiasts.  Make your own CF-PP filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.

Processing Recommendations:

  • Pre-dry before extrusion at 50°C for 4-6 hours.  PP-based materials typically don’t require pre-drying, but the addition of CF often leads to wicking of some moisture and pre-drying is recommended.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  160-190°C (depending upon how your heater bands, thermocouple, and PID are configured.)