PVA Water Soluble Support Pellets
Ideal for making your own filament or for use in a pellet-fed 3D printer.
Please note: Additional shipping charges may apply on orders over 10kg.
Processing Recommendations:
- Pre-dry before extrusion at 50°C for 4-6 hours. A toaster oven works fine for this. Do your family a favor and do not dry the resin in your kitchen oven! (Wet material will extrude with bubbles present in the filament. If this happens, dry the resin more before processing.)
- Extrusion Temp: 150 – 170°C depending on your extruder set-up.
- Do not cool using water tanks – this is a water soluble material and will dissolve in the water.