PSU Filament

 

Polysulfone (PSU) is an amorphous high-temp polymer and has higher thermal properties (Tg and HDT) than ULTEM™ 9085.  Our PSU is a great choice for demanding applications that require excellent thermal, mechanical, and chemical resistance properties.  

Print PSU with Gearbox™ HT2 High-Temp 3D Printer.  Check it out HERE.