Loading... Please wait...

CarbonX™ Carbon Fiber PLA 3D Printing Filament

Hover over image to zoom

  • Carbon Fiber PLA Filament
  • Carbon Fiber PLA 500g and 2kg Reels
  • Carbon Fiber Rocket - excellent surface appearance and light weight.
  • Image 4
  • Chopped Carbon Fiber
$38.00

 Product Description

CarbonX™ CFR Carbon Fiber Reinforced PLA Filament

CarbonX™ CFR-PLA is an improved CF reinforced 3D printing filament vs. the competition.  Made using High-Modulus Carbon Fiber (not carbon powder or milled carbon fiber).  This filament is ideal for anyone that desires a structrual component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing.  Made in the USA using premium Natureworks PLA and high modulus carbon fiber.  

NO heated bed required!  

CarbonX™ CFR PLA is suitable for use in practically any desktop 3D Printer.  Please note - carbon fiber reinforced filaments are abrasive and can wear out a brass or aluminum nozzle.  We recommend our A2 Hardened Steel Nozzles - HERE

New Data:  We updated the mechanical and thermal data on our carbon fiber grades.  You can see the new data HERE on our blog.

*Please note:  2kg and 4kg reels are special order and generally take 2-3 days to ship.  XL reel dimensions are 11.75" diameter, 4" wide, 2" arbor.  

1-3d-filament-technical-data.png

Recommended Print Conditions:

  • Extruder:  190-220°C.  
  • Bed Temp:  23 - 60°C  (Heated bed NOT necessary)  
  • Bed Prep:  3DXTech Blue Painters Tape, PVA-based Glue, Hairspray
  • Nozzle:  We currently recommend minimum 0.4mm orifice.  
  • Need a hardened nozzle?  Make sure to check out our A2 Hardened Steel Nozzles - HERE.  Our A2 hardened steel nozzles have 20X the wear resistance of brass! 

 Product Reviews

This product hasn't received any reviews yet. Be the first to review this product!

You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the CarbonX™ Carbon Fiber PLA 3D Printing Filament to your wish list.