Natural Transparent PC 3D Filament

3DXMAX® PC (Polycarbonate)

$46.00

3DXMAX® Polycarbonate (PC) 3D Printing Filament

3DXMAX® PC is a premium high-heat 3D printing filament made using Lexan® Polycarbonate from Sabic.  PC has some of the best mechanical properties & high-heat resistance in the 3D Printing world (Tg of 147°C).  Our PC allows for the printing of functional prototypes and production parts with very fine detail and excellent surface quality.  3DXMAX® PC is suitable for use in both consumer-grade and industrial FDM/FFF printers that have a heated print bed and extruders that can reach upwards of 300°C.   Made by 3DXTECH® in the USA.

Quantity:  500g (1.1lbs)

Filament Diameter Specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  280-310°C
  • Bed Temp:  110 - 120°C
  • Bed Prep:  ABS / Acetone Slurry on clean glass at 120°C works best for us.
  • Enclosure:   Although not 100% necessary, we recommend using a printer with an enclosure to help keep some heat in while printing with PC.
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.