Carbon Fiber PEEK Pellets

CarbonX® CF-PEEK Pellets


CarbonX® Carbon Fiber Reinforced PEEK - Pellets.

Ideal for home extrusion enthusiasts.  Make your own carbon fiber filament with a home-extruder such as the Noztek, Filabot and Filastruder.

Processing Recommendations:

  • Pre-dry before extrusion at 150°C for 4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  370-390°C