Firewire® Flame Retardant PC-ABS 3D Printing Filament
Firewire® Flame Retardant PC-ABS (polycarbonate + ABS alloy) is made using a premium UL94 V-0 rated PC-ABS. It has higher strength and thermal resistance (HDT) than ABS, alloying the mechanical properties and high-heat resistance of PC with the printability of ABS. This filament is ideal for applications which require UL94 V-0 self-extinguishing characteristics.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our FR PC-ABS and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations
Extruder Temp
265-285°C
Bed Temp
110-120°C
Heated Chamber
Recommended
Nozzle Specs
No special concerns
Bed Adhesion
Magigoo Bed Prep
Layer Height
No special concerns
Drying Specs 80°C for 6 hours
Supports
Water Soluble Supports
Benefits of Firewire Flame Retardant PC-ABS:
- Improved durability and sturdiness in parts with highly flame-retardant, self-extinguishing properties, superior to FR-ABS alone
- High thermal properties making it functional up to 110°C
- Easier to print than most industrial-grade materials
- Amorphous structure gives it lower, near isotropic shrinkage
- Made using UL94 V-0 rated base resin
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 265-285°C
- Bed Temp: 110-120°C
- Bed Prep: Magigoo Bed Prep gives us the best results
- Heated Chamber: Recommended, a chamber helps reduce warping and improves layer adhesion
- Supports: AquaTek™ water soluble X1 USM Universal Support Material is designed to work with complex models
- Drying Instructions: 80°C for 6 hours
Safety Note:
Direct ventilation is required to print Firewire Flame Retardant PC-ABS. This grade has a much more pronounced odor during printing and it is highly recommended to use in a well-ventilated area or with HEPA and carbon filtration systems available.