FibreX™ Nylon+GF30 30% Glass Fiber Reinforced Nylon
Our Nylon+GF30 glass fiber reinforced Nylon 6 Copolymer (PA6) is nothing less than an industrial-grade beast! Formulated to be exceptionally stiff and strong, all without being brittle. Polyamides (PA) are the work horse of the plastics industry the world over thanks to their excellent mechanical, chemical, and thermal resistance. The addition of heavy glass fiber reinforcement takes it to the next level.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our PA6+GF30 and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations
![FibreX PA6+GF30 Ext Temp 1 Ext Temp 1](https://www.3dxtech.com/wp-content/uploads/2021/01/Ext-Temp-1-1024x1024.jpg)
Extruder Temp
260-280°C
![FibreX PA6+GF30 Bed Temp Bed Temp](https://www.3dxtech.com/wp-content/uploads/2021/01/Bed-Temp-1024x1024.jpg)
Bed Temp
60-75°C
![FibreX PA6+GF30 Chamber Temp Chamber Temp](https://www.3dxtech.com/wp-content/uploads/2021/01/Chamber-Temp-1024x1024.jpg)
Heated Chamber
Not required
![FibreX PA6+GF30 Nozzle Settings Nozzle Settings](https://www.3dxtech.com/wp-content/uploads/2021/01/Nozzle-Settings-1024x1024.jpg)
Nozzle Specs
0.4mm diameter minimum
Hardened Steel Nozzle
![FibreX PA6+GF30 Bed Adhesion Bed Adhesion](https://www.3dxtech.com/wp-content/uploads/2021/01/Bed-Adhesion-1024x1024.jpg)
Bed Adhesion
Magigoo Bed Prep
![FibreX PA6+GF30 Layer Height Layer Height](https://www.3dxtech.com/wp-content/uploads/2021/01/Layer-Height-1024x1024.jpg)
Layer Height
0.25mm or higher
![FibreX PA6+GF30 Drying Filamen Drying Filamen](https://www.3dxtech.com/wp-content/uploads/2021/01/Drying-Filamen-1024x1024.jpg)
Drying Specs
90°C for 4 hours
![FibreX PA6+GF30 Water Soluble Support Water Soluble Support](https://www.3dxtech.com/wp-content/uploads/2021/03/Water-Soluble-Support-1024x1024.jpg)
Supports
X1 USM Water Soluble Support
Benefits of Nylon+GF30 Include:
- Printable on practically any 3D printer with a heated bed
- Ideal for structural engineering-grade applications
- Exceptionally stiff and strong, without being brittle
- Excellent chemical resistance makes it suitable for automotive and industrial applications
- Resists fuels, lubricants, heat, and mechanical loading
- High thermal properties keep it strong up to 170°C in use, depending on printing and mechanical loads applied
- Glass fiber reinforcement improves dimensional stability, reduces shrinkage, lift, and warp
- Very strong layer bonding
![FibreX PA6+GF30 ion chem resistance ion chem resistance](https://www.3dxtech.com/wp-content/uploads/2020/12/ion-chem-resistance.jpg)
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 260-280°C
- Bed Temp: 60-75°C
- Nozzle: We currently recommend a hardened steel nozzle with a minimum diameter of 0.4mm
- Other: Ideal layer height is 60% of nozzle diameter. We do not recommend printing layers smaller than 0.25mm with glass fiber reinforced filaments
- Bed Prep: Magigoo Bed Prep or 3DXTECH Polyimide Tape gives us the best results
- Heated Chamber: Not required, but a 30-80°C chamber does improve layer bonding and finished part mechanical properties
- Supports: AquaTek™ water soluble X1 USM Universal Support Material works ideal for complex parts.
- Drying Instructions: 90°C for 4 hours.
Glass Fiber Reinforced Filament
![FibreX PA6+GF30 Glass Fiber Zoom In Glass Fiber Zoom In](https://www.3dxtech.com/wp-content/uploads/2021/03/Glass-Fiber-Zoom-In-1024x1024.jpg)
What Is It?
Fibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament.
This, along with their physical makeup, give this material enormous strength and mechanical properties.
![FibreX PA6+GF30 GF Stiffness GF Stiffness](https://www.3dxtech.com/wp-content/uploads/2021/03/GF-Stiffness-1024x1024.jpg)
What Does It Do?
Glass fiber reinforcement gives material a lot of desirable properties:
- High strength
- High stiffness
- High chemical resistance
- Low thermal expansion
![FibreX PA6+GF30 GF Reel GF Reel](https://www.3dxtech.com/wp-content/uploads/2021/03/GF-Reel-1024x1024.jpg)
How Does It Work?
Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
![FibreX PA6+GF30 GF Part Vice GF Part Vice](https://www.3dxtech.com/wp-content/uploads/2021/03/GF-Part-Vice-1024x1024.jpg)
What Is It Good For?
Ideal for any applications which require strength and rigidity.
For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.
Abrasive Material
This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.