3DXMAX® PC-ABS 3D Printing Filament
3DXMAX® PC-ABS (polycarbonate + acrylonitrile butadiene styrene) is a premium high-heat 3D printing filament. PC-ABS alloys the mechanical properties & high-heat resistance of PC with the printability of ABS and allows for the printing of functional prototypes and production parts with very fine detail and excellent surface quality. 3DXMAX® Low-Gloss PC-ABS is suitable for use in both consumer-grade and industrial FDM/FFF printers that have a heated print bed. Made by 3DXTECH® in the USA.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our PC-ABS and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations
Extruder Temp
270-290°C
Bed Temp
110-120°C
Heated Chamber
Recommended
Nozzle Specs
No special concerns
Bed Adhesion
Magigoo Bed Prep
Layer Height
No special concerns
Drying Specs
110°C for 4 hours
Supports
Works best with
X1 USM Water Soluble Support
Benefits of 3DXMAX® PC-ABS:
- Sturdy parts with durable qualities from PC and printability from ABS
- Easier to print than Polycarb, yet tougher than ABS
- Improved thermal properties, ductility, and impact resistance
- Amorphous structure giving it lower, near isotropic shrinkage
- Beautiful low-gloss surface finish helps hide layer lines and makes highly technical-looking printed parts
Filament Specifications:
1.75mm and 2.85mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 270-290°C
- Bed Temp: 110-120°C
- Bed Prep: Magigoo Bed Prep Adhesive or 3DXTECH Polyimide Tape gives us the best results
- Heated Chamber: Recommended, a chamber helps reduce warping and improves layer adhesion
- Supports: Water soluble AquaTek X1 USM works ideal for complex parts.
- Drying Instructions: 110°C for 4 hours.