LTS2 Low-Temp Support Filament
LTS2 Break Away Support was developed for our Gearbox™ HT2 3D Printer. This material is specifically formulated as a break away support for ABS and ASA model materials. LTS2 is capable of supporting ABS and ASA in heated build chambers up to 100°C. Suitable for open-source printers with non-heated chambers and those with chambers up to 100°C.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our LTS Filament and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations

Extruder Temp
220-235°C

Bed Temp
85-100°C

Heated Chamber
Not required

Nozzle Specs
No special concerns
Benefits of 3DXMAX™ LTS2:
- Good adhesion to ABS and ASA
- Pre-programmed into the Gearbox HT2

Technical Data Sheet
This material doesn’t yet have a formal TDS.

Safety Data Sheet
This material doesn’t yet have a formal SDS.
Filament Specifications:
1.75mm +/- 0.05mm in diameter
Recommended Print Settings:
- Extruder: 220-235°C
- Bed Temp: 85-100°C
- Bed Prep: Magigoo Bed Prep gives us the best results.
- Heated Chamber: Not required
- Drying Instructions: No drying needed at all!