E3Dv6 Hercules A2 Hardened Steel Nozzle

E3Dv6 Compatible Hercules™ A2 Hardened Steel Nozzle

$28.00

E3Dv6 Compatible Hercules™ A2 Hardened Steel Nozzle

Hercules™ nozzles are manufactured in the USA by Performance 3D using heat treated A2 tool steel and coated with Duraplat3-d™ wear-resistant coating for enhanced wear and flow.  Compared to stainless steel nozzles, Hercules™ nozzles are 3X harder, have 50% better heat transfer, and 5x the wear life.  Hercules™ nozzles are the clear cut choice for printing with more abrasive filaments like our CarbonX™ Carbon Fiber grades.