ThermaX™ PEEK 3D Printing Filament [BLUE]

$375.00

ThermaX™ PEEK 3D Filament [BLUE]

ThermaX™ PEEK (PolyEtherEtherKetone) is one of the highest-performance polymers in world.  Our PEEK filament is made using a proprietary processing technique that allows for lower extrusion temperatures than other PEEK filaments on the market and is therefore easier to print with.  

PEEK has exceptional mechanical, thermal, and chemical resistance properties making it a go-to material in some of the most demanding applications.  The Polyaryletherketone (PAEK) family of thermoplastics exhibit exceptional thermal, chemical, and mechanical properties.  The PAEK family includes the following polymers:

  • Polyetheretherketone (PEEK)
  • Polyetherketoneketone (PEKK)
  • Polyetherketone (PEK)
  • Polyetherketoneetherketoneketone (PEKEKK)  

Product Attributes Include:

  • Glass Transition Temp (Tg) of 143°C 
  • Melt Temp (Tm) of 343°C 
  • Inherent flame resistance (UL94 V-0)
  • Outstanding mechanical, thermal, and chemical resistance
  • Continuous Use Temperature (CUT) of 260°C, higher for short duration
  • Excellent resistance to a broad range of chemicals, such as those used in the oil/gas, automotive, aerospace, industrial, and chemical processing industries

Filament Specifications:

  • Diameter:  1.75mm (+/- 0.05mm)
  • Color:  Blue

Recommended Print Conditions:

  • Extruder Temp:  375 - 410°C
  • Bed Temp: 130 - 145°C
  • Bed Prep: Ultem™ Tape is the ideal build surface, glue stick on clean glass is suitable
  • Enclosure temp (if your printer is equipped):  70 - 140°C [hotter is better, up to 140°C]
  • Print Speed:  10-50 mm/s for 0.2mm layer height, fast as results dictate

Victrex PEEK, Solvay Ketaspire PEEK, Evonik Vestakeep