BVOH Support

AquaTek™ BVOH Water Soluble Support Filament

$60.00

AquaTek™ BVOH Support Filament

Our BVOH is an advanced water-soluble support filament for printing complex parts.  BVOH (Butenediol Vinyl Alcohol Co-polymer) is water-soluble and is easily removed from the printed part with room-temp water.  AquaTek™ BVOH offers great adhesion to a wide range of materials, including PLA, ABS, PETG, and Nylon.  Extruded by 3DXTECH using state-of-the-art equipment at our plant in Grand Rapids, MI.  

Note:  Keep BVOH dry and store filament in the zip-lock mylar that is supplied with desiccant or in a sealed container with desiccant.  

AquaTek™ BVOH Attributes:

  • BVOH is readily soluble in water
  • Ideal support material for a wider array of materials (PLA, ABS, ASA, PETG, Nylon, Carbon Fiber)
  • Low moisture absorption while exposed during printing

Filament diameter specs:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder:  190-220°C
  • Bed Temp:  60-90°C