Support Filaments

We offer a variety of support including those that are water soluble and break away - all ideal for printing complex parts.  

  • AquaTek™ Water Soluble Support [BVOH and PVA]
  • 3DXMAX® HIPS Break Away Support
  • ThermaX™ High-Temp Break Away Support